Why do fine hairline scratches form on a lapped surface?
The fine scratches seen after lapping do not have a single cause. Unexpectedly coarse grains in the abrasive grain distribution, coarse abrasive from a previous operation remaining in the machine, burrs on the carrier edges, hard particles embedded in the plate, poorly cleaned samples, an incorrect film thickness or unsuitable pressure can all play a role to different degrees. Hard phases within the metal itself can also change the surface marks. When investigating the cause, the entire process chain should be examined first, not the name of the chemical used.
What can a large number of scratches at different angles indicate?
In double-sided systems, the workpiece is exposed to more than one direction of relative movement, so marks can appear in different directions. However, a large number of pronounced scratches beyond the normal kinematic marks may be caused by contamination with coarse particles or by a damaged plate or carrier. Questions such as whether the scratch distribution is uniform, whether it is concentrated in certain carrier pockets and whether every material gives the same result help with the diagnosis.
Why does clicking and carrier noise increase in the machine?
It should not be assumed that frequently repeated noise alone indicates a lack of abrasive. Carrier–gear clearance, incorrect carrier thickness, plate wear, load distribution, alignment, film thickness or damaged pockets should be evaluated. Adding fluid or abrasive may temporarily reduce the noise; this does not mean that the underlying mechanical cause has been eliminated. In the event of unusual noise, rubbing or signs of jamming, the machine should be stopped safely and inspected according to the manufacturer's instructions.
How can too much water, too little oil or low film strength cause problems?
The fluid affects the working behaviour of the moving surfaces and the abrasive. An unsuitable or over-diluted fluid can weaken the rust protection of metal surfaces; by changing the film conditions and the abrasive distribution, it can increase the risk of direct contact and friction. However, crushing of a carrier or damage to a plate cannot be definitively diagnosed simply by saying "too much water was added"; the mechanical load, the position of the part/carrier and the working clearance must also be examined.
Why is a stop needed after a carrier is crushed or the plate is scratched?
A damaged carrier can create new protrusions on its edges and dimensional deviation. Continuing to work with it can wear the workpiece and both working plates further. If there are deep marks on the plate that can be felt with a fingernail, the surface form, residues of foreign particles and mechanical alignment should be inspected by competent maintenance staff. Since random sanding or grinding of the surface can make the flatness even worse, the manufacturer's maintenance method must be followed.
Why can purplish or coloured marks appear on the surface?
Discolouration on steel can be caused by surface film residues, the chemistry of the process fluid, oxidation, insufficient rinsing, local temperature changes or optical reflections under lighting. Colour alone does not prove that the material has overheated or been metallurgically damaged. Especially on critical parts, whether the marks change with cleaning, the condition of the material and any possible thermal effect should be checked separately.
What happens if one side of the part is machined more than the other?
Different removal on the upper and lower surfaces can lead to undesirable results in terms of thickness, parallelism and surface texture. The causes may include a difference in condition between the upper and lower working surfaces, different contact pressure, a defective carrier, flow distribution or deflection of the part. The initial geometry also affects the results.
How can flatness deteriorate after lapping?
An unsuitable plate form, elastic deformation of the workpiece under pressure, excessive temperature differences, uneven abrasive distribution and poor seating of the part can cause local wear. Using a double-sided system alone does not mean that every part will be perfectly flat in every area.
Why is cleanliness a quality parameter?
With very small amounts of stock removal, even an uncontrolled metal chip or a coarse abrasive grain can be very large relative to the target surface texture. Workshop organisation, separate slurry containers, the process sequence, tool/carrier cleanliness and the workpiece washing procedure should be regarded as part of the quality plan.
Technical evaluation flow for the first sample
- The technical drawing and material are reviewed.
- The opposing surfaces to be processed are identified.
- The target thickness, parallelism, flatness and Ra/Rz requirements are separated.
- Safe placement of the part in the carrier is checked.
- The need for pre-processing is evaluated.
- Abrasive and fluid options compatible with the material are selected.
- A trial is carried out and the results are checked with a suitable method.
- If necessary, the parameters are revised.
- Once the acceptance criterion is clear, series production begins.