Causes of Scratches in Lapping

Abrasive contamination, carrier condition, plate flatness, fluid film and cleanliness factors that affect scratch formation in lapping.

When fine marks appear on a surface after lapping, the first suspect may be the abrasive grain size. In very fine surface finishing, however, even a small foreign particle is a significant factor. Residue from a previous coarse abrasive, metal chips, a worn carrier or a scratched plate can produce the same appearance. Reducing a problem to a single cause can therefore lead to a wrong diagnosis and unnecessary replacement of consumables.

For a reliable evaluation, the process should be examined step by step. The initial surface condition of the parts, the type of abrasive and fluid used, machine cleanliness, the mechanical condition of the carriers and the distribution of the marks should be recorded. On some surfaces, concentrated marks near the carrier may point to a mechanical guidance problem, while marks scattered over the whole surface may increase the likelihood of contamination; however, these observations alone are not a definitive diagnosis.

Moving to a finer abrasive only makes sense once the grains left from the coarse stage have been cleaned away. In addition, the surface should be evaluated not only visually but, where necessary, with a suitable profilometer and geometric measurements.

Let us review your part.

Send us your technical drawing and target surface requirements, and we will determine the right process together.

Get a Quote

How would you like to send your technical drawing?

What should the technical drawing include?Tap to see the 8 details we need, such as material, quantity, dimensions, tolerance and target Ra/Rz.