Skip to content
LeplemecimLeplemecim

Abrasives and process

Lapping Fluids and Process Parameters

Lapping slurry, lapping oil and emulsions; the effect of pressure, relative speed, temperature, stock allowance, plate condition and carriers on the lapping result.

What is an abrasive slurry?

A mixture in which loose abrasive grains are carried in a suitable fluid is called a lapping suspension or slurry. The fluid helps carry the grains to the working zone, regulate contact behaviour, remove heat and clean away residues at the end of the process. A slurry that is too dense, too thin or not homogeneous can affect the abrasive distribution and surface quality.

Lapping oil, soluble oil and water-miscible emulsions

Lapping oil refers to oil-based products formulated as a carrier fluid for specific abrasive and machine conditions. Soluble oil (known in Turkey as "bor yağı") is a broad market term for metalworking fluids that are usually mixed with water; it is not a single chemical formula. An emulsion may consist of a mixture of water and certain oil components; synthetic or semi-synthetic metalworking fluids work differently. The product's rust protection, foaming, biological stability, metal compatibility and behaviour with the abrasive should be evaluated according to its technical data sheet.

Why the choice of fluid matters

Cast iron lapping plates and iron-based carriers can be sensitive to the rust protection properties of water-based fluids. An incorrect water ratio, insufficient rust-inhibiting components, a dirty mixture left standing for a long time or a plate that remains dry can create a risk of corrosion and surface deterioration. Conversely, an oil film that is too heavy or unsuitable can also change the abrasion behaviour. For each product, the manufacturer's mixing range, water quality, pH, concentration and microbiological maintenance instructions must be taken into account.

Why should different oils not be mixed at random?

Fluids that are not compatible with each other can cause problems such as precipitation, foaming, reduced corrosion protection or uneven transport of the abrasive grains. High ratios such as "half oil, half water" may not match the range recommended for the product. A mixing ratio that has not been verified by the manufacturer should not be applied as a general process recipe.

Pressure and loading in lapping

The pressure applied to the part affects the behaviour of the abrasive on the surface and the fluid film thickness. Increasing the pressure does not always improve the surface; under certain conditions it provides higher removal but can increase the risk of scratches, plate contact or thermal effects. Too little pressure can result in insufficient processing or irregular contact. Suitable values are determined experimentally for the specific machine, part area, carrier and fluid conditions.

Rotational speed and relative speed

The speeds of the upper plate, lower plate and planetary carriers may be independent of each other or kinematically linked. What matters is not just the speed of one motor but the relative speed between the abrasive and the part and the distribution of the contact paths over the part surface. A higher speed can increase removal in some applications; however, it has limits such as heat, film breakdown, carrier instability and abrasive distribution. It cannot be said that "maximum speed is always best".

Temperature management

The heat generated during processing can temporarily change the dimensions of the metal part and the plate. Temperature differences can affect the reliability of measurement and the thickness/flatness results. In addition, an unsuitable metalworking fluid may not remove thermal effects sufficiently. With very tight tolerances, temperature equalisation after processing and the measurement environment are especially important.

Stock removal allowance

Before lapping, it should be clearly known how much material in total can be removed from which surface of the part. On parts that are already very close to the nominal size, heat treated or hard coated, the amount to be removed can be more critical. When two surfaces are machined together, the total thickness change is the sum of the removal from both surfaces. For estimating process time, sample data on the part material, surface area and actual removal rate are useful.

Plate condition and conditioning

The working surface of the lapping plate is one of the main factors affecting the flatness achieved on the part. Wear over time, local hollowing, marks, embedded coarse grains or hard dirt on the plate can worsen the result. The plate maintenance and conditioning method should be determined according to the machine/plate manufacturer's instructions. A plate that is not flat or is seriously damaged cannot be reliably compensated for simply by changing the abrasive.

Carriers (planetary carriers) and the ring gear system

In double-sided lapping and some precision two-surface machining systems, the carriers hold the workpieces in their pockets and, with a suitable design, travel around the machine while rotating about their own axes through a sun/ring gear mechanism. Carrier thickness, pocket clearance, material and gear compatibility can be critical. Bent, crushed or burred carriers should be checked, as they can cause new scratches, jamming and plate damage.

Why can the surface be matte grey after processing?

On some metal parts machined with loose abrasive on a cast iron lapping plate, light is scattered in different directions, which can produce a uniform matte or satin grey appearance. This can be the result of controlled lapping. Applications that require a mirror finish may need a different polishing method, finer abrasives or special processes. A matte grey appearance alone is not a negative sign for the functional quality of the surface.

Cleaning and particle control after lapping

Abrasive residues, metal chips and carrier fluid residues can cause undesirable wear in the part's working system. Cleaning after processing should be planned according to the part's material, geometry, sealing areas and subsequent assembly conditions. Dirty cleaning containers with mixed abrasives also carry a risk of contaminating subsequent fine lapping jobs. Proper separation, labelling and cleaning practices contribute to repeatability.

Let us review your part.

Send us your technical drawing and target surface requirements, and we will determine the right process together.

Get a Quote

How would you like to send your technical drawing?

What should the technical drawing include?Tap to see the 8 details we need, such as material, quantity, dimensions, tolerance and target Ra/Rz.